René® Superalloys (41, 80, 95)

René® superalloys are age-hardened nickel-chromium alloys that have high strength and are high-temperature and corrosion-resistant. They are suitable for use at both cryogenic temperatures as well as higher temperature use up to 1300 F.


René® 41 Chemical Composition
Cr= 18.00-20.00%, Ni= remainder, Mo= 9.00-10.50%, Co= 10.00-12.00%, Al= 1.40-1.80%, Ti= 3.00-3.30%, Fe= 5.00% max., plus other minor impurities
René 80: Ni= 60.0%, Cr= 14.0%, Co= 9.5%, Ti= 5.0%, Mo= 4.0%, W= 4.0%, Al= 3.0%, C= 0.17%, B= 0.015% and Zr= 0.03%


René® 80 Chemical Composition:
Ni= 60.0%, Cr= 14.0%, Co= 9.5%, Ti= 5.0%, Mo= 4.0%, W= 4.0%, Al= 3.0%, C= 0.17%, B= 0.015% and Zr= 0.03%

René®95 Chemical Composition
René 95: Ni= 61.0%, Cr= 14.0%, Co= 8.0%, Mo= 3.5%, W= 3.5%, Nb= 3.5%, Al= 3.5%, Ti= 2.54%, Fe= <0.3%, C= 0.16%, B= 0.01% and Zr= 0.05%
Typical Applications

Applications for René® alloys include gas turbine hot section components and cryogenic storage tanks.

Packaging Options

N/A

Classification

René® SuperalloysTSCA (SARA Title III) Status: Listed
Please contact the EPA Office of Chemical Safety and Pollution Prevention (OCSPP) at 202-564-2902.

Add René® Superalloys (41, 80, 95) To Your Quote

Select Specifications Available

  • René 41
  • René 80
  • René 88DT
  • René 95

Units

  • Pieces
  • Grams
  • Troy Ounces
  • Pounds
  • Kilograms
  • Metric Tons
  • Net Tons
  • Feet
  • Meters
  • Inches
  • Centimeters
  • Millimeters
Not seeing what you're looking for? Request Product

Do you supply materials similar to this product? Reade is always expanding its network with trusted suppliers. Partner with us to bring your products to our global client base.

Partner with Reade

Thank you for adding a product to your quote request!

Submit a RFQ

Review & Submit

View other Products

View Products